Melamine crosslinking agent. Percentage usage varies from 0.5 to 1% on the product to be crosslinked.
|
|
|
|
Crosslinking agent for solvent-based acrylic adhesives.
|
|
|
|
Melamine crosslinking agent to be added to the printing paste (2-3%) to improve resistance to washing and rubbing.
|
|
|
|
Polyfunction isocyanate crosslinking agent suitable for crosslinking of polymers with free OH groups. Percentage usage varies from 5% to 8% on the product to be crosslinked.
|
|
|
|
Melamine crosslinking agent for polyurethane resins with free OH groups. Percentage usage varies from 4% to 8% on the product to be crosslinked.
|
|
|
|
Catalyst to be used with melamine crosslinking agent Icaplink A520. Percentage usage varies from 0.5 to 1% on the product to be crosslinked.
|
|
|
|
Melamine crosslinking agent to be used in quantities varying from 0.3 to 0.8% on the polyurethane to be crosslinked .
|
|
|
|
Accelerator for Icaplink 75. Recommended percentage usage varies from 1 to 2% on the polyurethane to be crosslinked.
|
|
|
|
Melamine crosslinking agent for polyurethanes with free OH groups. Percentage usage varies from 4 to 8% on the product to be crosslinked.
|
|
|
|
Aliphatic polyisocianate easily dispersible in water based PU and acrylic dispersions. The amount to apply is dependant on the structure of the polymer and is ranging from 1% to 5%. Pot-life is influenced by the reactivity of the system and by pH.
|
|
|
|
Crosslinking agent for products in aqueous dispersion containing carboxylic groups. Suggested amount to use: from 1% to 5% of polymer. Pot-life is dependant on pH (longer at high pH) and temperature. Never use after 24 hours from mixing.
|
|